Printing on a P2S, I adjusted the top layer slightly from 0.42 to 0.5, slowed the ironing speed from 30mm/s to 20mm/s, and adjusted the ironing flow from 30 to 35%. This gave a smoother finish on the faces and helps keep the red one from looking a little pink (the white top layer is really thin). The designs are great. I appreciate the plate setup to minimize color changes! Printed them all in PLA Basic.